We have had a customer request information on the solderability shelf
life of untreated copper SMT pads (no OSP, HAL, Ni/Au, etc.). Is there a
study or report showing the solderability overtime of untreated copper
pads? Any ideas on how to activate untreated copper for solderability
prior to assembly?
***************************************************************************