Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0wAMGJ-000BkSC; Thu, 27 Mar 97 14:59 CST |
Content-Type: |
text/plain; charset=us-ascii |
Old-Return-Path: |
|
Date: |
Tue, 26 Mar 1996 23:07:31 +0000 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
MIME-Version: |
1.0 |
Status: |
O |
X-Mailing-List: |
|
From [log in to unmask] Thu Mar 27 15: |
56:08 1997 |
TO: |
|
Return-Path: |
<TechNet-request> |
X-Status: |
|
Resent-Message-ID: |
<"8Evii1.0.r8M.M-jEp"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
Content-Transfer-Encoding: |
7bit |
X-Mailer: |
Mozilla 3.01 (Win16; I) |
Message-ID: |
|
Parts/Attachments: |
|
|
Hello,TechNetters!
Consider please the following problem:
Let's say,you have an expensive multilayer board with a nicked
conductor.The nick narrows the conductor to 50%,but there is no
problem concerning electrical performance.
Would you cosider repair with a welded covar strip?
Our supplier suggested the repair,but after seeing the mess around
it,I would much more prefer to use the board as it is.
Does anybody support this?
Thank you,
Gaby
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|