Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0wAHhx-000Bj2C; Thu, 27 Mar 97 10:07 CST |
Content-Type: |
text/plain; charset=us-ascii |
CC: |
|
Old-Return-Path: |
|
Date: |
Thu, 27 Mar 1997 10:18:27 -0800 |
Precedence: |
list |
Reply-To: |
|
Resent-Sender: |
|
MIME-Version: |
1.0 |
Status: |
O |
X-Mailing-List: |
|
TO: |
|
X-Status: |
|
Return-Path: |
<TechNet-request> |
X-Loop: |
|
Resent-From: |
|
From [log in to unmask] Thu Mar 27 11: |
08:49 1997 |
Content-Transfer-Encoding: |
7bit |
Resent-Message-ID: |
<"A7N3f2.0.PwJ.uifEp"@ipc> |
Subject: |
|
From: |
|
References: |
|
X-Mailer: |
Mozilla 3.0 (Win16; U) |
Organization: |
Circuit Research |
Message-ID: |
|
Parts/Attachments: |
|
|
Darrell Daigle wrote:
>
> Hello technetters, I will try this for the fifth time,I apologize if your
> file is loaded with this request, it has been returned to me as undelivered
> mail.
>
> If a gold finger with splashes of tin/lead on it "does not" make contact
> within a gold socket, will there be galvanic corrosion.
> Unfortunately IPC-A-600 does not address reliability issues, if there is
> reference material out there, I would like to know.
Hello All:
Along similar lines I have observed select corrosion of solder occurr
during the resist stripping process, but only solder connected to gold
tabs. It was presumed a galvanic corrosion was taking place but the
"pathway" of this corrosion has not been identified. Perhaps anyone
with an answer to the above question could shed some light on this
problem as well. Thanks for your assistance!
Regards,
Ted Stern
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|