Received: |
from simon.ipc.org by vnet.IBM.COM (IBM VM SMTP V2R3) with TCP;
Wed, 12 Mar 97 02:33:39 EST
from ipc.org by simon.ipc.org via SMTP (940816.SGI.8.6.9/940406.SGI)
id BAA24399; Wed, 12 Mar 1997 01:23:10 -0800
by ipc.org (Smail3.1.28.1 #2)
id m0w4YvC-000BEdC; Tue, 11 Mar 97 15:17 CST |
Encoding: |
7 TEXT |
TO: |
|
Old-Return-Path: |
|
Date: |
Tue, 11 Mar 97 16:28:00 PST |
X-Loop: |
|
Precedence: |
list |
Resent-From: |
|
Message-ID: |
|
Resent-Message-ID: |
<"oxqT7.0.IiF.NlS9p"@ipc> |
Resent-Sender: |
|
From: |
|
Subject: |
|
X-Mailing-List: |
|
X-Mailer: |
Microsoft Mail V3.0 |
Resent-Date: |
Wed, 12 Mar 1997 01:23:10 -0800 |
Parts/Attachments: |
|
|
Hello Technetters,
I am having a slight problem with the amount of solder on fiducials. This is
causing optical recognition problems during the pick and place.
Any suggestions, maybe an alternative surface finish.
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|