Lynette,
I don't know exactly what type of information that you are
looking for, but IPC-A-610B Section 6.0 covers "marking acceptability
requirements". If you are looking for the silkscreen or stamping
"process" then you might reference IPC-A-600 or IPC-D-275. Hope this
helps.
Dwight Nolen
Manufacturing Quality Engineer/QA Supervisor
Frontier Engineering
Stillwater, Oklahoma
405-624-5329
______________________________ Reply Separator _________________________________
Subject: marking standards
Author: PC:[log in to unmask] at INTERNET
Date: 3/25/97 1:04 PM
Hi,
Can anyone tell me if there is an IPC standard for silkscreen
and board markings? If so where can I find it?
Thanks
Lynette Hawkins
Tektronix, INC.
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|