See SMI proceedings, Sept 1996, p650
Chris Hunt
___________________ Forwarded Message _____________________
Date: Fri, 21 Mar 97 17:31:00 GMT
From: Yuen, Mike
To: [log in to unmask]
Subject: Mechanical Properties: Intermetallic Thickness!
Related question on mechanical properties!
Are there any publications out there documenting the adverse impact(s) of
excessive intermetalic growth of Eutectic Solder (Not Gold Embrittlement
just regular Cu3Sn and Cu6Sn5)?
Thanks
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|