Hi TechNetters.
I wonder if anybody out there has encountered the following:¨
I have seen plastic resdues on LCCC pads, probably coming from the black
ESD-sticks that the components arrive in. If I rub the LCCC or the stick
on a piece of white paper it turns black. I can also see the residues on
LCCC:s using a microscope.
I hope my problem has already been solved somewhere.
Thanks
//