TECHNET Archives

March 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0w34SL-000BF9C; Fri, 7 Mar 97 12:33 CST
Old-Return-Path:
Date:
Fri, 7 Mar 1997 11:41:00 -0600
Precedence:
list
Resent-From:
From [log in to unmask] Mon Mar 10 08:
27:52 1997
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/10943
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"EVEch3.0.ty9.rz58p"@ipc>
Subject:
From:
Steve Masear-RVG230 <[log in to unmask]>
X-Loop:
X-Mailer:
Worldtalk (4.1)/STREAM
Message-Id:
<M992920.001.oryd0.1.970307184212Z.CC-MAIL*/OU=52CC8/OU=AZAC/PRMD=MOT/ADMD=MOT/C=US/@MHS>
Parts/Attachments:
text/plain (75 lines)
IS THIER ANY INFORMATION ON GOLD WIREBOND RELIABILITY TO ANY PALLADIUM METAL
SYSTEM?  WHAT ARE THE METAL SYSTEMS, AND WHAT ARE THE THICKNESSES?


The information may be old but two papers were presented at the 1983
NEPCON West.  One was titled "How much gold is enough for electronic
interconnections" by Will Reyes at Xerox. The other was "Palladium-
Nickel as an alternative to Gold in connector applications" by Undegraff
and Graham at du Pont.  Some data regarding porosity, HNO3 testing,
contact resistance, etc is included in the papers.  I would be happy to
share this information with you if you feel it is of any use.
 ----------
From: es500yap@pts7
To: [log in to unmask]
Subject: FAB: Palladium Plating
Date: Friday, March 07, 1997 5:00AM



Does any have any experience with Pd plating replacing Selective Au &
ENIG
on
PWB?  Are there any success stories? Is there any data collected on the
reliability of this plating? What is the plating thickness like for Ni,
Pd?
 Is
Au in the content?  If yes, how much?

 Appreciate any input.


 regards,
 stella

************************************************************************
***
* TechNet mail list is provided as a service by IPC using SmartList
v3.05 *
************************************************************************
***
* To subscribe/unsubscribe send a message <to: [log in to unmask]>
 *
* with <subject: subscribe/unsubscribe> and no text in the body.
 *
************************************************************************
***
* If you are having a problem with the IPC TechNet forum please contact
 *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]
 *
************************************************************************
***

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2