TECHNET Archives

March 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0w2QNF-00080SC; Wed, 5 Mar 97 17:45 CST
Content-Type:
text/plain; charset=us-ascii
Old-Return-Path:
Date:
Wed, 05 Mar 1997 17:52:19 -0500
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
MIME-Version:
1.0
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/10883
TO:
IPC TechNet <[log in to unmask]>
Return-Path:
<TechNet-request>
X-Status:
X-Loop:
Resent-Message-ID:
<"PgsLg3.0.7fK.OMW7p"@ipc>
From [log in to unmask] Thu Mar 6 14:
31:16 1997
Subject:
From:
Robert Boilard <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Message-ID:
Organization:
Everything P.C.
X-Mailer:
Mozilla 3.0Gold (Win95; I)
Parts/Attachments:
text/plain (26 lines)
I have a problem with adhesive squeeze out on single sided flex layer.
My drilled hole size is .053" and I have squeeze out that is closing
done the hole done to .043".  We have tried plasma etch to to get the
acrlyic out of the hole, but because there is no through hole (only
coverlayer access hole)  plasma is not working.  Is there a way to
remove the adhesive from the pads without having to skive all of them.

My panel size is 12x18 and I 74 sheets plus many strips that were die
cut from other panels...

Appreciate all who reply....

Thank You

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2