Hello,
At the burn in operation, we sometimes find a green stuff as well as black
stuff that look like corrosion and they're located under the conformal
coating. When analysing the stuff, it came out as copper chloride for the
green spots and copper sulfide for the black spots. Any idea as to where
they could originate from ?
Thank you.
***************************************************************************