TECHNET Archives

March 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0w9d9e-000BlIC; Tue, 25 Mar 97 14:49 CST
Encoding:
7 TEXT
Old-Return-Path:
Date:
Tue, 25 Mar 97 16:04:00 PST
Precedence:
list
Resent-From:
Message-ID:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11467
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"-IK7Y1.0.lyA.9f3Ep"@ipc>
Subject:
From:
Darrell Daigle <[log in to unmask]>
X-Loop:
Resent-Sender:
TechNet-request [log in to unmask]
X-Mailer:
Microsoft Mail V3.0
From [log in to unmask] Tue Mar 25 15:
00:14 1997
Parts/Attachments:
text/plain (20 lines)

Hello technetters,

If a gold finger with splashes of tin/lead on it "does not" make contact 
within a gold socket, will there be galvanic corrosion.
Unfortunately IPC-A-600 does not address reliability issues, if there is 
reference material out there, I would like to know. 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2