Mime-Version: |
1.0 |
Content-Type: |
text/plain; charset="us-ascii" |
Old-Return-Path: |
|
Date: |
Mon, 3 Mar 1997 18:39:21 -0600 (CST) |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
X-Sender: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Loop: |
|
Resent-Message-ID: |
<"3yuzW3.0.eZG.Bqs6p"@ipc> |
Subject: |
|
From: |
|
From [log in to unmask] Tue Mar 4 08: |
49:02 1997 |
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0w1i7I-0007zYC; Mon, 3 Mar 97 18:30 CST |
X-Mailer: |
Windows Eudora Pro Version 2.2 (16) |
Message-Id: |
|
Parts/Attachments: |
|
|
At 12:04 PM 3/3/97 -0800, you wrote:
>I would appreciate some guidance on a subject that could be of interest
>to others in the same dilemma.
>
>We are specifying controls for unpopulated PWB's to be used in low
>residue/no clean process. We plan to restrict bare board bulk ionic
>levels to no more than 2 micrograms/sq.in. NaCl equivalent. Also, it
>has been suggested that we require that 'polyethylene glycol substances,
>as well as certain dry film and even some liquid photoimageable masks be
>avoided'. The bulk ionic requirement is easy to communicate but I am
>struggling with the verbiage and test methods that describe restrictions
>on polyethylene glycol substances and other potentially harmful
>materials.
>
>Any help in this matter will be greatly appreciated.
>
>Mary Davis
>Sr. Material & Process Engineer
>Hughes Aircraft
>Naval & Maritime Systems
Mary,
I cannot answer your question regarding wording for PEG's, etc., (Were still
working on that one...) but I would like to caution you about relying
exclusively on bulk ionics. We have had a similar specification for some
time, and have had boards which exhibit excessive electrical leakage at
elevated temperature and humidity while passing bulk ionics test. I would
suggest that if the following conditions apply to your product, you should
use ion chromatography in conjunction with insulation resistance
measurements to characterize the acceptable levels of specific contaminants
for your designs.
1.) Your products have circuits with impedances in excess of 100 Megohms
2.) Your requirements for product performance are stringent (higher than 50
C and/or 90% RH)
I'd be happy to provide more information off-line.
Regards,
Fritz Byle
Sr. Process Engineer
Rockwell Automation
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|