TECHNET Archives

March 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Tue, 04 Mar 1997 01:21:47 +0200
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/10813
X-Sender:
[log in to unmask] (Unverified)
TO:
Return-Path:
<TechNet-request>
X-Loop:
Resent-Message-ID:
<"RcMQY2.0.4CC.8hr6p"@ipc>
Subject:
From:
From [log in to unmask] Tue Mar 4 08:
48:40 1997
Received:
by ipc.org (Smail3.1.28.1 #2) id m0w1gtt-0007zYC; Mon, 3 Mar 97 17:12 CST
X-Mailer:
Windows Eudora Pro Version 2.2 (32)
Message-Id:
Parts/Attachments:
text/plain (34 lines)
Gerry,
You asked about our findings regarding resin recession.

We treat resin recession according to MIL-P-55110D (I don't remember which
paragraph) that allowed the following: 
- Resin recession on Max. 50% of the dielectric hole wall on "as received"
samples. 
- Unconditioned resin recession after thermal shock.

We hardly ever see resin recession on "as received" boards and we see a very
low extent (less then 10-15%) recession on samples after thermal shock.
What I must add to this is that we are working with an IR reflow process
(not  HASL) and that most of our multilayer boards are polyimide.

Hope that it helps,
Yehuda Weisz
    ************************************* 
    *          Yehuda E. Weisz              *
    *  e-mail: [log in to unmask]   *
    *  Tel: 972-3-5240362                    *
    ************************************

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2