Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0w6E7p-000BBhC; Sun, 16 Mar 97 05:29 CST |
Content-Type: |
text/plain; charset=iso-8859-1 |
CC: |
|
References: |
|
Date: |
Sat, 15 Mar 1997 19:31:00 -0500 |
Precedence: |
list |
Reply-To: |
|
Resent-Sender: |
|
MIME-Version: |
1.0 |
Status: |
O |
X-Mailing-List: |
|
X-Sender: |
|
TO: |
|
X-Status: |
|
Return-Path: |
<TechNet-request> |
X-Loop: |
|
Resent-From: |
|
Content-Transfer-Encoding: |
8bit |
Old-Return-Path: |
|
Resent-Message-ID: |
<"V-TY31.0.e68.CczAp"@ipc> |
Subject: |
|
From: |
|
From [log in to unmask] Mon Mar 17 17: |
06:31 1997 |
X-Mailer: |
Mozilla 3.01 DT [de]C-DT (Win16; I) |
Organization: |
TAUBE ELECTRONIC |
Message-ID: |
|
Parts/Attachments: |
|
|
K.Varadaraj@CADET, India. wrote:
>
> Hello
>
> I would like to know if fabricating an SMD (double side mount), Six layer
> PCB, which has a 50 mil pitch pin to pin and 100 mil pitch row to row, 44
> pin connector, is possible any where. The drill provided is 30 mil and the
> pad is 32mil x 80 mil, oblong. Six mil track is routed between the pins.
>
> We have had a vendor fabricate this board here in India and due to process
> tolerances, the yeild is very less or almost has been nil.
>
I recommend the following:
1. choose a smt-connector instead of a drilled one.
2. Donīt route traces between the pins. Because of the total fabrication
tolerances of 8-10 mil and layer misregistration the risk of shorts
between drilled holes and adjacent traces on inner layers is very high.
Rainer Taube
TAUBE ELECTRONIC
http://www.taube-electronic.de
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|