TECHNET Archives

March 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
From [log in to unmask] Mon Mar 10 11:
47:58 1997
Old-Return-Path:
Date:
Mon, 10 Mar 97 11:34:05 -0500
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
Content-Transfer-Encoding:
7bit
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/10988
TO:
Return-Path:
<TechNet-request>
X-Status:
Resent-Message-ID:
<"DBXEc2.0.2eC.lz39p"@ipc>
Subject:
From:
"Harlan Vince"<[log in to unmask]>
X-Loop:
Received:
by ipc.org (Smail3.1.28.1 #2) id m0w48WG-000BBwC; Mon, 10 Mar 97 11:05 CST
X-Mailer:
ccMail Link to SMTP R6.0
Message-Id:
Parts/Attachments:
text/plain (56 lines)

     Yes,  You can also plate with OSPs and Hard/TAB gold.  This works very 
     well if you are utilizing Gold/Card Edge Connectors or something 
     similar that requires a gold contact surface.  
     
     Ni/Au PWBs in wave solder or SMT reflow solder very well.  We limit 
     the Au thickness to 2-6 microinches (very important).  We have 
     experienced some "peculiarities" in wave solder but not directly 
     attributed to Ni/Au PWBs.  For some reason a Ni/Au PWB does not 
     tolerate touchup or post-wave assembly as well as a HASL or OSP PWB.  
     Maybe someone more knowledgeable on this topic can shed some 
     additional light. 
     
     Harlan


______________________________ Reply Separator _________________________________
Subject: Selective PCB plating
Author:  <[log in to unmask]> at INTERNET
Date:    3/10/97 9:49 AM


Does anyone know if you can selectively plate with OSPs and Immersion 
gold on the same PCB?  I would like to do immersion gold on my keypad 
contacts but use something Like Entek on the rest of the PCB.  Is this 
possible?  
     
My PCB assembly vendor doesn't like reflowing immersion gold PCBs.  He 
claims the solder doesn't flow very well.  Is it just him or the rest of 
the industry?
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     
     


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2