Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0w48C2-000BC4C; Mon, 10 Mar 97 10:44 CST |
From [log in to unmask] Mon Mar 10 11: |
47:08 1997 |
Old-Return-Path: |
<Victor_Johansen@coates> |
Date: |
Mon, 10 Mar 97 07:22:34 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"C03YV1.0.VHG.9g39p"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
Resource error - try resending
Original text follows
-----------------------------------------
Received: by ccmail
Received: from goodnet by coatesasi.com (UUPC/extended 1.11) with UUCP;
Mon, 10 Mar 1997 07:21:27 MST
Received: from simon.ipc.org ([168.113.24.64]) by ns1.goodnet.com (8.8.5/8.6.9) with SMTP id GAA07497 for <[log in to unmask]>; Mon, 10 Mar 1997 06:58:14 -0700 (MST)
Received: from ipc.org by simon.ipc.org via SMTP (940816.SGI.8.6.9/940406.SGI)
id HAA16168; Mon, 10 Mar 1997 07:42:38 -0800
Resent-Date: Mon, 10 Mar 1997 07:42:38 -0800
Received: by ipc.org (Smail3.1.28.1 #2)
id m0w44oz-000BBrC; Mon, 10 Mar 97 07:08 CST
Resent-Sender: [log in to unmask]
Old-Return-Path: <simon.ipc.org!pop.eunet.ie!hormann!Maurice_Dore>
Message-ID: <[log in to unmask]>
X-Charset: MACINTOSH
To: [log in to unmask] (technet)
From: [log in to unmask] (Maurice Dore)
Date: Mon, 10 Mar 1997 13:19:44 GMT
Subject: Gen- Cu protective coating
Resent-Message-ID: <"ATt4q3.0.a17.bV09p"@ipc>
Resent-From: [log in to unmask]
X-ccAdmin: postmaster@goodnet
X-Mailing-List: <[log in to unmask]> archive/latest/10973
X-Loop: [log in to unmask]
Precedence: list
Resent-Sender: [log in to unmask]
Date 10/3/97
Subject Gen- Cu protective coating
From Maurice Dore
To technet
Gen: Cu protective coating
quality
11:45 10/3/97
hi all
I have used a test to determine the imidazole based protective coating on Cu
by applying ferric chloride to the Cu (Ref: IPC-TM-650 2.3.22)
The result has shown a tarnish in different areas of the pads.
Does anyone out there use this test to check the coating on the Cu?
THANKS
MOSS
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|