Wenesco makes the lowest cost spray fluxer that I would buy. They're
located in Chicago.
Making your own will run into the following problems:
Ventilation
Overspray is messy
Spray pattern is critical to yield and coverage
Drip is an issue
....etc.
______________________________ Reply Separator _________________________________
Subject: spray fluxing, VOC free
Author: [log in to unmask] at internet
Date: 2/4/97 10:19 AM
I have an electrovert 10" machine with a single platten preheater, I would like
to change over to VOC free flux. I know that I need more evaporation for the
water. I figure that my options are the following:
New machine --$$??@@!!
Spray Fluxing - will help by reducing the flux present in the first place
Convective preheat - need more hot dry air to remove H2O
I have probably 18" that I could add convective preheat in, which would give me
an overall preheat length of 27", which is not all that much, but combined with
convective dry air, this might be enough.
Can anybody give me some direction on building a spray fluxer?
We are presently using Kester 951 which generally works well, but I have seen
better soldering with the VOC free if I can make the process work, and I won't
have to accumulate the spent alcohol flux.
Peter Roy
Broy Engineering Ltd
Toronto
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|