Subject: | |
From: | es500yap@pts7 ( YAP CHOW LAN) |
Date: | Fri, 28 Feb 1997 13:19:12 +0800 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Does any have any experience with Pd plating replacing Selective Au & ENIG on
PWB? Are there any success stories? What is the plating thickness like for Ni,
Pd? Is Au in the content? If yes, how much?
Appreciate any input.