have had this promlem befour and it has alot to do with the design
of the board, and the catalyst and or HCL acid bath prior to the
catalyst. We change our HCL very frequently and we run at 20%.
If you need to talk to the expert in eletroless NI. AU. email me
and I will give you a name and phone number to call.
kyle w. gulley