It would seem that I have a problem that some other people get from time to time
no mail. Have I been removed from the list ??

Has the USA closed for business ?

Bob Willis
Process Engineering Consultant
Electronic Presentation Services
2 Fourth Avenue, Chelmsford, Essex CM1 4HA. England.
Tel: (44) 01245 351502
Fax: (44) 01245 496123
Home Page: http://ourworld.compuserve.com/homepages/Bwillis
Email: [log in to unmask]


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2