Brett,

Waterbourn solder mask is not a real new technology.  I know Coats/ASI has
had a waterbourn mask for years, and I beleave that Peters also has one also.
 When I tested waterbourn mask, back about 3 years ago, it had viscosity
problems, but I'd think that the bugs should be worked out by now.

Let me know if I can be more help.

Scott. 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2