TECHNET Archives

February 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Wed, 5 Feb 1997 18:18:10 -0500
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
From [log in to unmask] Mon Feb 10 08:
39:52 1997
X-Sender:
TO:
Return-Path:
<TechNet-request>
X-Loop:
Resent-Message-ID:
<"aZ2uM.0.l18.mRK-o"@ipc>
Subject:
From:
[log in to unmask] (Jack Crawford)
X-Mailing-List:
<[log in to unmask]> archive/latest/10003
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vsJus-0000XVC; Wed, 5 Feb 97 20:50 CST
Cc:
Message-Id:
<v01540b17af1e7e6dc41a@[204.180.62.40]>
Parts/Attachments:
text/plain (113 lines)
More info on this from the good folks at NIST. Jack
------------
Date: Wed, 05 Feb 1997 16:32:53 -0500
From: [log in to unmask] (Ursula_Kattner_x6044)
Subject: Re: Alloy contamination
To: [log in to unmask]
Cc: [log in to unmask], [log in to unmask],
        [log in to unmask]

>A phase diagram for Ag-Pb-Sn is published in: P. Villars, A. Prince
>and H. Okamoto, "Handbook of Ternary Alloy Phase Diagrams" Vol.3,
>ASM International, Materials Park, OH, 1995.  In this book the
>sources of the diagrams are given as A. Prince et. al., private
>communication, and three more references.
>The system has a ternary eutectic L = Ag3Sn + (Pb) + (Sn) at 180 C
>with a liquid composition of 1.5 wt.% Ag, 35.0 wt.% Pb (1.9 at.% Ag,
>23.5 at.% Pb), the compostions of the solid phases can be assumed
>to be identical to the corresponding binary systems.
>The addition of Sn will lower the liquidus and solidus approximately
>with the same slopes as in the Sn-Pb binary system.  Simultaneous
>addition of Pb will decrease the effect.  It should be noted that
>the solidus for the given composition is the (Pb) + Ag3Sn tie-line.
>The equilibrium ternary ternary eutectic begins to form when the
>the tie-line of Sn-saturated (Pb) + Ag3Sn is crossed.  However, due
>to the effects of non-equilibrium solidification (segregation) the
>ternary eutectic may be observed earlier.
>
>Hope this information helps,
>Ursula R. Kattner
>Metallurgy Division, Materials Science & Engineering Laboratory
>Bldg. 223, A153
>NIST,  Gaithersburg, MD 20899
>Phone: 301-975-6044       Fax: 301-975-4553
>e-mail: [log in to unmask]

>
>|  From [log in to unmask]  Wed Feb  5 14:40:57 1997
>|  Date: Wed, 05 Feb 1997 14:38:59 -0500
>|  From: Carol Handwerker <[log in to unmask]>
>|  Subject: Re: Alloy contamination
>|  X-Sender: [log in to unmask]
>|  To: [log in to unmask]
>|
>|  Please respond to this person who has a question about the effect of tin
>|  additions on liq. and sol. temps.    Thanks.
>|  Carol
>|
>|  >Return-Path: <[log in to unmask]>
>|  >Date: Wed, 5 Feb 1997 13:54:39 -0500
>|  >X-Sender: [log in to unmask]
>|  >To: [log in to unmask]
>|  >From: [log in to unmask] (Jack Crawford)
>|  >Subject: Re: Alloy contamination
>|  >Cc: [log in to unmask], [log in to unmask]
>|  >
>|  >Following from the EMPF Helpline, prepared by our metallurgist John=
>|   Greaves:
>|  >
>|  >Increasing the Sn content will lower the liquidus and solidus, and once the
>|  >Sn content increases beyond a point (I am not sure what that point is) a
>|  >low melting binary eutectic phase will form ( eutectic SnPb, melts at
>|  >183=B0C).  The person to ask about this is Carol Handwerker at NIST.  Her
>|  >phone is 301-975-6158, and her email is :    [log in to unmask]
>|  >
>|  >
>|  >If she can't help you then your answer doesn't currently exist.
>|  >
>|  >Hope this helps,
>|  >
>|  >John Greaves
>|  >
>|  >----------
>|  >>From: [log in to unmask]
>|  >>Date: Wed, 5 Feb 1997 07:08:08 -0600
>|  >>To: <[log in to unmask]>
>|  >>Subject: ASY: Alloy contamination
>|  >>
>|  >>
>|  >>Here's one for the metallurgist. I have been unable to locate a
>|  >>Pb93.5/Sn5/Ag1.5 (305C liquidus; 309C solidus) ternary phase diagram
>|  >>to date. I have been told that one of the technical issues is simply
>|  >>soldering to SnPb plated and/or SnPb hot-dipped coated components with
>|  >>this PbSnAg solder will realize a drop in the melting point. My
>|  >>question is how much ? Assuming, for instance a lead finish
>|  >>composition of Sn63/Pb37 with solder coat thickness of 3 to 4 mils or
>|  >>a CERDIP package with leads that are 100% Sn electroplated (200 to
>|  >>500micons).
>---------------------------------------------------------------

***ALL NEW EMPF PHONE NUMBERS***

Jack Crawford, HelpLine Coordinator
Electronics Mfg. Productivity Facility
****NEW--317.655.3688
****FAX  317-655-3699
714 N Senate Ave, Suite 100
Indianapolis IN  46202-3112
VISIT OUR HOME PAGE AT: http://www.empf.org
[log in to unmask]


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2