Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0w0FZv-0007zWC; Thu, 27 Feb 97 17:49 CST |
Old-Return-Path: |
|
Date: |
Thu, 27 Feb 97 17:19:00 CST |
Precedence: |
list |
Resent-From: |
|
Message-ID: |
|
X-Status: |
|
Status: |
O |
From [log in to unmask] Fri Feb 28 08: |
57:17 1997 |
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"KOxzh2.0.ugD.EsX5p"@ipc> |
Subject: |
|
X-Priority: |
3 (Normal) |
X-Mailing-List: |
|
X-Loop: |
|
Resent-Sender: |
|
From: |
|
Parts/Attachments: |
|
|
How much of EMF change after aluminum is anodized (chromated) depends on
how good/thick the coating is. It is fairly easy to measure the relative
potential delta of two materials. Check the book "Corrosion Engineering"
by Fontana/Greene or any other electrochemistry book and you'll know how to
do it. Remember, (1) surface area is an important factor, (2) Redox
(reduction/oxidation) potential is only a thermodynamic indicator, i.e.,
the tendency to corrode. It does not provide kinetic information, i.e.,
how fast it corrodes.
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|