TECHNET Archives

February 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vw7w0-0000SBC; Sun, 16 Feb 97 08:51 CST
Old-Return-Path:
Date:
Sun, 16 Feb 1997 10:00:51 -0500 (EST)
Precedence:
list
Resent-From:
From [log in to unmask] Tue Feb 18 12:
52:11 1997
Message-ID:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/10288
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"n5bhy.0.lC8.dxn1p"@ipc>
Subject:
From:
X-Loop:
Resent-Sender:
TechNet-request [log in to unmask]
Parts/Attachments:
text/plain (19 lines)
Please advise what your electrolyte is, normally we are used to seeing either
fluoborates, or Methane Sulfonates, and the potential answers to your
problems could be different depending on the electrolyte in your plating
bath.

Rudy Sedak

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2