First of all I stay with the "Class 3 Military" , internal .002, external .004.
What you need to know is, what size tool is my vendor using to achive
the called out finished hole size?
For a plated through hole:
MAX. ACCEPTABLE HOLE DIA. +.003" = (MAX TOOL SIZE)
MIN. ACCEPTABLE HOLE DIA. +.008 = (MIN. TOOL SIZE)
EX: PTH .028" +/- .003" (MAX. TOOL = .034") (MIN. TOOL = .033")
Now I need a list of avable tool sizes from my vendor(s) and a find the
max. tool that they would/could use. (.033") and plug that into this
formula:
Min. Pad = (AR + .005") x 2 + Drill Size
EX: .002" AR = (.002" + .005") x 2 + .033" = .047" PAD
Clear as mud?
Dan Lorinser
BFGoodrich Aerospace
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|