What information can anyone provide concerning brushing loose leads
and flags from circuit card assemblies and the preventative measures
to prevent electrostatic discharge (ESD) when using the brush provided
to clean off leads? We have had several ESD failures related to the
brushing action to clean off leads after the Q-Corp has cut the leads.
1. Has anyone any experience you could share?
2. What preventative measures have been taken to prevent ESD
failures?
***************************************************************************