I would be concerned about bringing the resin above it's Tg for this
length of time in an unsupported fashion. If the boards were just in a
rack you may be inviting warp. If they were stacked under weight this
may not be a problem. I would suggest for safety's sake having this
board built on FR-4 with a minimum Tg 170. This material is very
readily available.
On Feb 4, 12:03am, Ulrich Korndoerfer wrote:
> Subject: PCBs at 150°C for more than 2 hours
> Hi TechNetters!
>
> We use a multilayer pcb made from basically FR4 with a Tg of 135°C.
> There are pths, blind microvias, buried vias and some fine line wiring
> (only on top and bottom). One of our processing steps in building up
the
> assembly (after smd-soldering both sides and cleaning) is die attach
> with an adhesive. The recommended curing cycle of the adhesive is 1 h
> (actual it may be 2h ore more) at 150°C and is done in a convection
oven
> under normal atmosphere.
>
> I am interested in the cons of above curing temperature and time. Are
> there any reliability issues concerning the pcb? To my knowledge,
> laminating the pcb's by the manufacturer is done at even higher
> temperatures (although under vacuum).
>
> Any comments are welcome.
>
> Ulrich Korndörfer
>
>
************************************************************************
***
> * TechNet mail list is provided as a service by IPC using SmartList
v3.05 *
>
************************************************************************
***
> * To unsubscribe from this list at any time, send a message to:
*
> * [log in to unmask] with <subject: unsubscribe> and no text.
*
>
************************************************************************
***
> * If you are having a problem with the IPC TechNet forum please
contact *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]
*
>
************************************************************************
***
>
>
>-- End of excerpt from Ulrich Korndoerfer
--
Thomas Ingham
Eastern Regional Sales Mgr.
Details Inc.
714-630-4077
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|