Hi, Phil,
What kind of components in the Thru-hole process you may want to protect?
Would you need a similar kind of protection in the SMT reflow?
Thanks in advance.
Vic
On Mon, 17 Feb 1997 [log in to unmask] wrote:
> Here's one for you.
> Some time ago, a company sent me a sample of a material they had developed
> that could be used to shield heat sensitive components during reflow. It
> would be molded to conform to the surface geometry of the portion of the
> assembly to be protected. I'm a bit skeptical about whether it really works
> but I'd like to try it. It could be very beneficial for the Reflow Of
> Through-hole process applications.
> If anyone knows who this company is or where they are, please let me know.
> I'd like to experiment with the material.
>
> Phil Zarrow
> ITM, Inc.
> [log in to unmask]
>
> ***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> ***************************************************************************
> * To subscribe/unsubscribe send a message <to: [log in to unmask]> *
> * with <subject: subscribe/unsubscribe> and no text in the body. *
> ***************************************************************************
> * If you are having a problem with the IPC TechNet forum please contact *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
> ***************************************************************************
>
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|