We have used both Polyclad and Allied Signal's RCC (resin coated
copper) for laser drilling, and it is very successful. The
thickness of the resin we used was 50um/50um Cstage/Bstage, and we
ended up with minimum dielectric seperation of 80um between copper
foil and the 1/2 oz track on layers 2 and n-1.
Dougal Stewart
Exacta Circuits
Scotland
***************************************************************************