Dave;
The IPC design rules have certainly taken this spacing into account. The
IPC-D-275 requires that the designers add a "Standard Fabrication Allowance"
per table 5-10. This table is intended to allow for variation in the
fabrication process. The amount of allowance chosen, should be placed in a
note on the master drawing, flagging the amount to the fabricator,
inspection, and purchasing.
If the inspection allows breakout beyond the incorporated allowance, then
there could very well be a spacing violation to the nearest conductor.
I mention purchasing, since it is their job to match vendor capabilities with
design requirements. No sense sending a job to a fabricator that is beyond
his normal capability.
Regards,
Gary Ferrari
IPC Staff
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|