Mime-Version: |
1.0 |
Content-Type: |
text/plain; charset="iso-8859-1" |
Old-Return-Path: |
|
Date: |
Wed, 5 Feb 1997 14:12:13 +0100 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
Content-Transfer-Encoding: |
quoted-printable |
Status: |
O |
X-Mailing-List: |
|
X-Sender: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Status: |
|
X-Loop: |
|
Resent-Message-ID: |
<"AXA-6.0.M39.-o8-o"@ipc> |
From [log in to unmask] Wed Feb 5 09: |
24:43 1997 |
From: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vs7W3-00004ZC; Wed, 5 Feb 97 07:35 CST |
Subject: |
|
X-Mailer: |
Windows Eudora Light Versión 1.5.2 |
Message-Id: |
|
Parts/Attachments: |
|
|
To Victor.
Hi Victor,
I've readed your question. Please find here enclosed different alloys with
low meelting point, that my company manufactures:
67Sn 33Cd....176ºC
66,5Sn 29Cd 4,5Zn....158ºC
50Sn 32Pb 18Cd....145ºC
60Bi 40Cd....144ºC
60Sn 40Bi....138-170ºC
57Bi 43Sn....138ºC
56Bi 40Sn 4Zn....130ºC
55,5Bi 44,5Pb....124ºC
55Bi44 Pb1Sn....117-120ºC
54Bi 26Sn 20Cd....103ºC
52,5Bi 32Pb 15,5Sn....96ºC
52Bi 40Pb 8Cd....92ºC
50Bi 25Pb 12,5Sn 12,5Cd....70-72ºC
49,5Bi 27,5Pb 13Sn10Cd....70ºC
Concerning pricesor additional informatio, as Technet is a technical forum,
I preffer you will contact me by fax, or directly to my E-mail.
Best regards
=============
ANTONI CHERTA
(Barcelona)
Ph:+34.07.20.49.42
Fx:+34.3.274.00.80
E-mail: [log in to unmask]
=====================
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|