TECHNET Archives

February 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII; name="Stainless"
Old-Return-Path:
Date:
Wed, 19 Feb 97 08:56:54 +0100
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
Content-Transfer-Encoding:
7bit
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/10355
TO:
Return-Path:
<TechNet-request>
Content-Disposition:
inline; filename="Stainless"
X-Status:
X-Loop:
Resent-Message-ID:
<"QGRJ_2.0.Gt9.u3h2p"@ipc>
Subject:
From:
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vx6oD-0000VhC; Wed, 19 Feb 97 01:51 CST
X-Openmail-Hops:
1
From [log in to unmask] Wed Feb 19 12:
13:10 1997
Message-Id:
<H000032400b7c853@MHS>
Parts/Attachments:
Stainless (32 lines)
Dear Technetters.

We have been trying to solder a connector of plated stainless steel to a
ceramic substrate. We have not been sucessful so far.
Cracks occur in the solder joint after soldering.
We think the coefficient of thermal expansion in the stainless steel is
to high.
The material in the connector is CRES 303. (Acc to ASTM 484 and 582)
What material is the connector made of? The supplier is an american
company.

The CRES 303 says nothing to me.
Is the material an ordinary 18-8 stainless steel (18%NI and 8%Cr)?
In that case the coefficient of thermal expansion is approx 18 ppm and
that could explain the cracks.

Regards
Christer Marklund
 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2