TECHNET Archives

February 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Sat, 15 Feb 1997 13:54:12 -0600 (CST)
Precedence:
list
Resent-From:
From [log in to unmask] Tue Feb 18 12:
46:16 1997
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/10282
X-Sender:
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"zl7YV.0.Y_7.e3X1p"@ipc>
Subject:
From:
David Arivett <[log in to unmask]>
X-Loop:
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vvpxH-0000VhC; Sat, 15 Feb 97 13:39 CST
X-Mailer:
Windows Eudora Light Version 1.5.4 (16)
Message-Id:
Parts/Attachments:
text/plain (24 lines)


  An article in the February edition of PCFAB talks about laser drilled
micro-vias. It shows a multi-layer stack-up of two cores with pre preg in
the center. The outer layers are formed with resin coated foil. My question
is: how thick is the resin on the foil? I am sure it must be at least 2 mils
in order to have enough resin to encapsulate the inner layer circuitry. What
is the maximum it might be?

David Arivett
Cuplex Inc.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2