I use a CyberOptics Laser Section Microscope to measure solder paste
height on boards. It can also be used to measure length and width and
hence be used to measure misregistration. They can be reached at
(612) 542-5000.
Linda Kenison
Senior Process engineer
Vicor
(508)749-7570
______________________________ Reply Separator _________________________________
Subject: measuring paste height
Author: [log in to unmask] at Internet
Date: 1/31/97 8:03 AM
Can anyone reccommend a manufacturer of a device that measures
the height of solder paste after it is applied to the board.
+
Thanx Ahead
+
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************