Help!
I am designing flexible circuits that seem to be over the IPC-D-275 charts.
Or any of the current capacity charts being that they are all the same. I
have circuits that utilize a ARINC 600 size 3 connector with insert A,D
having 150 x #22 AWG, B,E 60 x #20 AWG, and C,F 100 x #22 AWG.
My problem is with the "Input Current", The 22 AWG circuits are to carry
a current of 3 AMPS and the 20 AWG are to carry 5 AMPS. The hole
pattern for the 22 AWG is on 0.100" centers with a .035" hole and a
.065" pad, leaving .035" spacing. The 20 AWG pattern is on 0.150"
centers with a .043" hole and .073" pad, leaving a .077" spacing. First, a
question with the charts, is a rigid flex considered an internal layer?
Are any flexes considered internal becouse of a kapton cover coat,
and/or a stiffener material? If considered internal, and I use a high TG
material (Polyimide), could I not go higher than the 45 deg C rise above
ambient? How? Also, in IPC-D-275 pg.10, note 5 states that for "groups
of similar parallel..." isn't that really the same as note 4? I do NOT know
how many of these circuits will be "on" at the same time and for how
long in time. I would think that if I put even 3 amps into parallel circuits
acording to the internal chart: 3 amp at 45 deg C rise, with 2 oz copper
equals a .030" trace (I have room for a .020" trace) that my flex would
heat up past that point. Now the 5 amp lines! Am I missing the boat? Is
there another way?
Dan
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|