     SANJAY,
     
     THERE ARE TWO JEDEC STANDARDS FOR QFP'S.
     
     MS-022; MQFP WITH BODY THICKNESSESS 2.0MM AND GREATER; COPLANARITY IS 
     0.1MM.
     
     MS-026; TQFP WITH 1.0 AND 1.4MM BODY THICKNESSES; COPLANARITY IS 0.1MM 
     FOR 0.65MM LEAD PICH AND >..  0.08MM FOR 0.5MM LEAD PITCH AND <..
     
     MAURY


______________________________ Reply Separator _________________________________
Subject: GEN: Lead Coplanarity Spec??
Author:  [log in to unmask] at smtp
Date:    1/22/97 10:53 AM


     
Technetters:
     
I have a couple of questions and would appreciate 
any input...
     
1. What is the JEDEC/IPC spec on lead coplanarity
    for QFP's?
     
2. Can anyone recommend any tinning houses that would
    tin surface mount packages for us?  I know one such place 
    is Corfin, are there any other popular ones?
     
     
Thank you
     
________________________________________________ 
Sanjay Rajan        RF Communications Division 
Harris Corporation  Product Design Engineering 
1680 University Avenue   Phone:    (716) 242-3923 
Rochester, NY 14610 Fax: (716) 242-3174 
________________________________________________
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2