Jim Reed wrote:
> 
> Pratap, immersion tin coatings will loss their solderability in less than 24
> hours.  You may be able to use very aggressive fluxes and solder to immersion


PRATTA ELECTRONIC MATERIALS INC. -MANCHESTER -N.H. 
TEL: 603-6278488  FAX: 603-6278799
ARE NOW MARKETING A NEW TIN IMMERSION CALLED:"OMIKRON", 
THE SOLDERABILITY IS PROVEN TO BE  1 YEAR.(PASSED TEST OF AGEING
4 HOURS AT 155c.

IT CREATS NO WHISKERS.


YISRAEL LESHMAN
OCTAVA MARKETING
	ISRAEL
[log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2