Todd,
Havce you done cross sections of the soldermask coverage? Perhaps the spray
coater is not depositing a uniform coat and thin areas are being attacked.
[log in to unmask]
"Todd Rogers" <[log in to unmask]> Wrote:
|
| Technetters,
| We have been experiencing some sporadic problems with
| soldermask being
| burned off the edge of the circuits at the hot air level
| process. The
| soldermask on the knee of the trace seems to burn off and
| allows the solder
| to stick to the trace edge. We are using a chemical clean
| process prior to
| soldermask, and are spraying the soldermask on with a
| Teledyne spray
| coater. Has anyone else experienced these problems and
| what did you do to
| fix it?
|
| Todd Rogers
| PC Boards, Inc.
| [log in to unmask]
|
| **********************************************************
| *****************
| * TechNet mail list is provided as a service by IPC using
| SmartList v3.05 *
| **********************************************************
| *****************
| * To unsubscribe from this list at any time, send a
| message to: *
| * [log in to unmask] with <subject: unsubscribe> and
| no text. *
| **********************************************************
| *****************
| * If you are having a problem with the IPC TechNet forum
| please contact *
| * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at
| [log in to unmask] *
| **********************************************************
| *****************
|
|
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|