Subject: | |
From: | |
Date: | Fri, 10 Jan 97 13:42:26 CST |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
this is "Epoxide cellulose paper core, epoxide glass cloth surfaces copper-clad
laminated sheet of defined flammability (vertical burn test)." - the title of
the IEC 249-2-9 specification. FV 0 is the flammability rating which appears
equivalent to UL 94V-0.
______________________________ Reply Separator _________________________________
Subject: IEC 249-2-9-FVO-EP-CP
Author: [log in to unmask] at smtplink
Date: 1/10/97 1:16 PM
Can anyone tell me what this material (IEC 249-2-9-FVO-EP-CP) is?
Is it FR4, CEM1 etc
Thanks.
Tom Killick
CIT
510 829 0154
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|