     I use a thermally conductive epoxy from Epoxy Technology (930-4)  It 
     is a two part system but has excellent strength.


______________________________ Reply Separator _________________________________
Subject: ASSY: thermocouple adhesive
Author:  [log in to unmask] at Internet
Date:    1/9/97 12:32 PM


     
Can anyone recommend an easy to use, one part instant adhesive for attaching 
thermocouples to BT epoxy and FR-4  PCBs (for thermal profiling work)? I 
remember others using a Loctite product in the past but I don't remember the 
type. The adhesive only has to last about 10 runs through the oven.
     
Thanks
Don Foster
[log in to unmask]
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2