Jan:
Could you provide some additional data. What type machine are you
using? What conveyor speed? What is your top side board temperature?
What type fluxing unit are you using (i.e. . .wave, foam, or spray?).
Do you use any mask on your boards, like peelable mask or other
types? How accurate is your adhesive dot placement?
Ron Hollandsworth
ITT A/CD
[log in to unmask]
***************************************************************************