A request from lareau at Georgia Tech was posted on TechNet for
directions to literature on reliability issues and failure modes of
plastic packages (non-hermetic). If you want to pursue this matter,
you would do well to discuss it with Dr. Noel Donlin at Army MICOM,
Redstonne Arsenal, AL (not too far from you). Dr. Donlin has
expressed a great concern for the long-term reliability of plastic-
encapsulated microcircuits in military systems, and will be able to
give you some of the background info you might not see in print. You
can call him at 205-842-0156.