Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vn1rn-0000YFC; Wed, 22 Jan 97 06:33 CST |
Old-Return-Path: |
|
Date: |
Wed, 22 Jan 1997 07:42:39 -0500 (EST) |
From [log in to unmask] Thu Jan 23 13: |
41:52 1997 |
Precedence: |
list |
X-Loop: |
|
Message-ID: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"1ssTv1.0.t77.FaWvo"@ipc> |
Subject: |
|
From: |
|
Resent-From: |
|
Resent-Sender: |
|
Parts/Attachments: |
|
|
<< We need to provide 100% moisture seal on the top surface of some FR-4
boards
about 8"x12" that have SMT components mounted. Can I do this "easily"
in-house without much equipment? What materials and suppliers? We could
easily install a fume hood if necessary. This is not a high volume project.
What do I do about sealing vias?
thanks, Crawford Byxbee >>
Crawford,
There is no such thing as a 100% moisture seal with conformal coatings. All
of them are organic polymers, which have varying levels of moisture
permeability. Water WILL get through, it is only a matter of when. Better
to ask the question of why you feel you need to have a 100% moisture seal.
Of the available coatings, you should probably try a silicone (type SR)
coating or parylene coating. Since your volume is low, sending the product
off for parylene coating, avoiding capital investment, may be your best bet.
You might also consider a contract conformal coater.
Doug Pauls
CSL
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|