Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vkGi5-0000UoC; Tue, 14 Jan 97 15:47 CST |
Encoding: |
64 TEXT |
Old-Return-Path: |
|
Date: |
Tue, 14 Jan 97 15:56:00 CST |
Precedence: |
list |
Resent-From: |
|
Message-ID: |
|
X-Status: |
|
Status: |
O |
From [log in to unmask] Tue Jan 14 16: |
30:28 1997 |
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"I58LX2.0.xGF.Cy_so"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
X-Mailing-List: |
|
X-Mailer: |
Microsoft Mail V3.0 |
Resent-Sender: |
|
Parts/Attachments: |
|
|
Hi John,
I concur with you.
* Please refer to IPC-SM-782 Page 20 Figure 3-9.
(Preferred component orientation for SMT parts)
Hope that helps
Michael Yuen
----------
From: TechNet-request
To: Jan.Merstrand; technet
Subject: Re: WAVE SOLDERING SMT ICS
Date: Tuesday, January 14, 1997 9:42AM
> Hi John,
> I'm sorry, but i disagree with you on one thing. Of course if your'e
> adding "robber pads" and rotate the ic 90 deg it sure work without
> getting any bridging.
> But if you can't add any pads? Then i would do as i described using a
> chip-wave, ofcourse, in a nitrogen wave solderer. I it find most logical
> to run the ic with standard pads this way, then ofcourse i don't have
> alot of experience in soldering smt with a wave solderer, but i've been
> there.
>
> Jan Merstrand
> Wave Soldering Technician
>
Jan,
Our process engineers tested multiple land patterns and orientations
and came to the conclusion that I had listed. The pad sizes for our
wave solder library are different than for reflow. In other words
they optimized. You may be correct in that standard reflow pads in
the orientation you described is less prone to skips and/or bridging.
Someone else have an opinion?
---------------------------
John Laur
Rockwell Automation
Allen-Bradley Co Inc.
1201 South Second Street
Milwaukee, WI 53204
+1 414 382 2162 (fax)
+1 414 382 2393 (phone)
[log in to unmask]
---------------------------
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|