Hello fellow TechNetters:
Recently I had some questions regarding Phototool dimensions. I want to
thank all who responded. Your input was very helpful!
In the development of Silver Halide film, there are byproducts of spent
developer and fixer. How do you handle these? Or, more specifically...
I am told by some people, that depending upon the amount of silver in the
developer, if it is within limits, can be sent down the drain with the rinse
water. A waste treatment lab tech suggested that it could be used to treat
some of the waste they handle to adjust the pH. Has anybody tried re-using
spent developer for anything? Currently, the developer is drained from the
feed-and-bleed system of the Film Processor unit into a barrel, which is
carried to our Waste Treatment department.
In addition, how do you handle the spent fixer solution? It is usually
heavily concentrated with silver. Currently, it is drained from the
feed-and-bleed system of the Processor unit into barrels, which are carried
to Waste Treatment department, who sells the barrels. We have looked into
silver recovery units, but haven't found one we like (got any suggestions?).
I'd like to eliminate the handling chemical waste by our Artwork Generation
technicians. How do most places handle the by-products of Silver Halide film
development?
Thank you in advance.
Sincerely,
Process Engineer
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|