John,
Derik Fritsch (408-982-0161) at Beam On should be able to help you on the
NC610.
Which Kester No-clean pastes did you use and why do you want to switch to
Florida Cirtech?
We are in the process of qualifying Kester's NC830 paste and 951 liquid
flux. I am very interested in
knowing some of your past solderpaste history with the Kester no-cleans.
Thanks.
Ava Fung
Process Engineering, Trimble Navigation
-----------------------------------------
Address,
Has anyone had any experiences in using Florida Cirtech's water
soluable WS120A and WS130A and No-Clean NC610 solderpastes? I would
like to know any pros and cons of using these pastes. Our past
solderpaste history has been with the Kester No-cleans. I'll be
running some pilot test with the WS130A soon. Thank you.
John Gulley - QA
**************************************************************************
*
* TechNet mail list is provided as a service by IPC using SmartList v3.05
*
**************************************************************************
*
* To unsubscribe from this list at any time, send a message to:
*
* [log in to unmask] with <subject: unsubscribe> and no text.
*
**************************************************************************
*
* If you are having a problem with the IPC TechNet forum please contact
*
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]
*
**************************************************************************
*
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|