One method is to utilize the TGA (Thermogravimetric Analysis) or
reference the IPC-TM-650 Method 2.6.3
D.Drake
Sperry-Sun Drilling Services
______________________________ Reply Separator _________________________________
Subject: Unidentified subject!
Author: [log in to unmask] at Internet-Mail
Date: 1/21/97 12:37 AM
>Message was resent -- Original recipients were:
To:
[log in to unmask]
--------------
Dear technet users,
How do we find out the amount of moisture content in a printed circuit
board
Regds
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************