we have trained a number of operators to use no-clean flux and the
time was about 2 hours which most of the time was spent in having the
operator using the solder to get use to the way it reacts. in regard
to the requirements of j-001 the best is to train to 610 which covers
all the requirments of 001. this class takes about 2 to 3 days
depending on the skill level of the operator.
______________________________ Reply Separator _________________________________
Subject: Time to train operators: J-STD-001 and LRNC flux
Author: [log in to unmask] at _internetcc
Date: 1/7/97 12:26 PM
Technetters:
I'd be interested to hear how long it takes to train an operator (who
is used to working to military soldering standards) the operator-
related parts of J-STD-001 (i.e., acceptance requirements). I'd also
like to hear how long it takes to train an operator (who is used to
working with RMA flux) to solder using a low-residue no-clean flux.
Gordon Davy
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|