Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0vhHk2-0000WYC; Mon, 6 Jan 97 10:17 CST |
Old-Return-Path: |
|
Date: |
Mon, 06 Jan 97 08:25:42 PST |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
Resent-Message-ID: |
<"STckr.0.2UK.XMIqo"@ipc> |
Subject: |
|
From: |
|
From [log in to unmask] Mon Jan 6 10: |
45:32 1997 |
X-Loop: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
I used to see this problem at a former company. I attriubuted it to
an agressive microetch/solderstrip undercutting the mask and allowing
a thin piece of soldermask to be removed during the tapetest.
But since I have not spent years studying soldermask, I can't say for
sure..
What type of solder strip do you use?? We used Peroxide Biflouride
which probably a bit more aggressive than a standard Nitric.
______________________________ Reply Separator _________________________________
Subject: Solder Mask Peel Off
Author: [log in to unmask] at corp
Date: 1/3/97 7:29 PM
Friends:
We encounter a problem with solder mask peel off which is near gold
finger, while after gold plated.
Is there anybody experience to this problem solution ?
Our solder mask in use is "Tamura" & "Taiyo". Gold plating tank is deep
type.
Thanks and Best Regards,
Gloria Electronics, Taiwan
R & D Chief
Hawk Chen
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|