Andy,
Is it important for the solder mask to be a dry film? You may be able to
consider a liquid photoimageable soldermask. The Electra Polymers EMP110
Carapace has passed the ASTM-E-595-93 outgassing spec for space.
Van Miller
Electra Polymers
[log in to unmask]
***************************************************************************